Abstract

Utilization of EFB-derived biochar in sintering of iron ore has been conducted in this work with regards to the porosity of iron sinter. EFB has been heated up in argon atmosphere to 450°C in order to produce biochar. In the present work, the sintering process was conducted at 1150°C with variations of biochar content from 5% to 10%. In this case, the apparent density for iron sinter shows significant decrease as the biochar addition increase. The porosity of iron sinter showed a gradual increment from 5% to 7.5% and escalated at 10% biochar content. The results of porosity and apparent density were in line with the micrograph of iron sinter.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.