Abstract
Samples of a Ti6Al4V alloy were treated by thermochemical gas nitriding at 1120°C for 7 h. Gas nitriding provided formation of titanium nitride layer with a hardness over 1800 HV. The titanium nitride layer exhibited excellent wear resistance along with a lower coefficient of friction against alumina ball under dry sliding conditions when compared to the as-received state.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.