Abstract
The purpose of this work was to quantitatively describe the interconnected porosity in iron compacts, both in macro- and microscale. Size and volume fraction of micro-, meso- and macropores were examined in the compacts with density within 5˙6–6˙4 g cm−3, made in laboratory conditions of two iron powders: NC100˙24 and ASC100˙29 manufactured by Höganäs Company. The interconnected porosity was determined using the method based on measuring the sorption isotherms of CO2 and benzene at T=25°C in static conditions in a high vacuum gravimetric appliance equipped with McBain–Bakr weighers.Volume distributions of individual size classes of micro- and mesopores in the compacts made of both iron powders with fixed density were compared.Relationships between density and the interconnected micro- and macroporosity of the examined compacts were determined.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.