Abstract
The thermodynamic stability and phase transformation energetics of a tempered 9Cr–1Mo steel have been studied using drop and isochronal differential scanning calorimetry techniques. The measured enthalpy reveals a steep increase with temperature, especially for temperatures exceeding 650 °C. It is found that the emergence of various phases as a function of temperature has been clearly marked by the presence of distinct inflections in the measured enthalpy increment versus temperature curve, obtained using drop calorimetry. The isochronal differential scanning calorimetry experiments yielded precise values for the transformation arrest points. The ferromagnetic to paramagnetic transformation temperature is found to be about 740 ± 5 °C. The austenite start (Ac 1) and finish (Ac 3) temperatures recorded during continuous heating are found to be strongly dependent on the heating rate and the extrapolated, so called zero scan rate values are found to be 830 and 870 ± 5 °C, respectively, for Ac 1 and Ac 3. The process of cooling from austenite field yielded martensite for the cooling rates 5–40 °C min −1 employed in the present study. The martensite start temperature is fairly independent of the cooling rate and is found to be 370 ± 5 °C. By adopting a phenomenological model for calculating the enthalpy of metastable ferrite at temperatures higher than its known range of stability, the enthalpy change associated with austenitisation (α-ferrite + carbide → γ-austenite) transformation has been estimated as a function of temperature. It is found that in the temperature range 625–1200 °C, the variation of the enthalpy with temperature due to phase change can be considered to be linear, which in effect renders a constant value for the effective transformation specific heat. This value is found to be of the order of 15.4 J mol −1 K −1 (±8%) in the temperature interval, 650–1200 °C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.