Abstract

The fresh and used EUROCAT II V 2O 5–WO 3/TiO 2 catalysts have been studied by electron paramagnetic resonance. For both samples, V 4+ in clusterlike arrangement and two sites corresponding to VO 2+ ions in octahedral symmetry axially distorted were found. It has been shown that the TiO 2 phase transformation (anatase → rutile) occurs at lower temperature (1073 K) for the EUROCAT II catalysts than the WO 3/TiO 2 support. Impurities of Fe 3+ ions were detected both on the catalysts and on the WO 3/TiO 2 support. Q-band measurements have allowed a difference in the environment of the Fe 3+ ions caused by the SCR process to be observed. Finally, traces of Ti 3+ ions in the anatase phase have been detected.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.