Abstract
The technology of modification of textile mixed materials using carbon and zirconium targets has been developed. A change in the structure of a composite material based on a 07C11‑KV mixed fabric (produced by Mogotex OJSC) modified with carbon and zirconium clusters after exposure at low temperatures (up to ‑40 °C) in a climatic chamber was investigated. It is shown that at temperatures ‑20 – ‑30 °C, the material is de‑fibrous. At ‑40 °C, there is no de‑fibering, fiber straightening is observed. The continuity of the coating is maintained for all test variants.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Litiyo i Metallurgiya (FOUNDRY PRODUCTION AND METALLURGY)
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.