Inside a ladle there is one component of the material that often gets damaged, namely the Holding Magnet Type LS50, which has corrosion (damage) on the surface due to temperatures that reaches 1500 °C with a time limit of 150 minutes. Test shows the material contained in the Holding Magnet Type LS50 are steel, copper (CuZn), and magnet. The Steel of Holding Magnet Type LS50 has a chemical composition with the main ingredient of iron (Fe) around 97.961% and other elements such as carbon, silicon, manganese, chromium and other alloy elements. As for the microstructure, CuZn has a microstructure in the form of an α (alpha) phase and a s (betha) phase. The average of Holding Magnet hardness test results shows only CuZn experienced a very drastic decrease in the hardness value due to continuous heat exposure while the temperature for CuZn melting point is only 1084 ° C. Keywords: Chemical Composition, Metallography, Hardness. DOI: 10.7176/CMR/12-7-08 Publication date: October 31st 2020

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.