Abstract
AbstractA resorcinol resin/water dispersion and a rubber latex are added to 1% 2,2,6,6,‐tetramethylpyperidine‐1‐oxyl (TEMPO)‐oxidized cellulose nanofibers (TEMPO‐CNFs) dispersed in water, followed by oven drying at 40 °C for 20 h to prepare a dried TEMPO‐CNF/resorcinol resin/latex rubber (DTRL) mixture with a weight ratio of 1/0.5/3. DTRL is then added to a nitrile‐butadiene rubber (NBR) or a carboxy group‐containing NBR (X‐NBR) sheet, and the mixture is kneaded by a two‐roll mill at 20–30 °C with high shear forces. The tensile strength and Young's modulus of the crosslinked DTRL/rubber composite sheets remarkably increased from 10 and 12 MPa, respectively, for the reference sheet to 24 and 82 MPa, respectively, for the DTRL/rubber composite sheets containing ≈10 vol% TEMPO‐CNFs. Scanning electron microscopy revealed that no TEMPO‐CNF agglomerates are present in the DTRL/rubber composite sheets. The tensile properties of the composite sheets are the best when a X‐NBR sheet and NBR latex are used as the matrix rubber and latex in DTRL preparation, respectively. When water‐extracted DTRL (WDTRL, mass recovery ratio ≈94%) is used in place of DTRL, the WDTRL/rubber composite sheets show sufficient water resistance, while the tensile properties are almost the same as those of the DTRL/rubber composite sheets.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.