Abstract

Abstract Nanocelluloses occur under various crystalline forms that are being selectively used for a wide variety of high performance materials. In the present work, cellulose fibers (CF-I) were mercerized by alkaline treatment (CF-II) without molar mass variation (560 000 g/mol) and both were acid hydrolyzed, forming cellulose nanocrystals in native (CNC-I) and mercerized (CNC-II) forms. This work establishes detailed characterization of these two nanoparticles morphology (light and neutron scattering, TEM, AFM), surface chemistry (zetametry and surface charge), crystallinity (XRD, 13C NMR), and average molar mass coupled to chromatographic technics (SEC-MALLS-RI, A4F-MALLS-RI), evidencing variations in packing of the crystalline domains. The crystal size of CNC-II is reduced by half compared to CNC-I, with molar masses of individual chains of 41 000 g/mol and 22 000 g/mol for CNC-I and CNC-II respectively, whereas the same charged surface chemistry is measured. This fundamental analysis may give insight to new applicative development.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.