Abstract

The paper presents an improved method of manufacturing cellular glass using residual glass (91 %), sodium borate (5 %), eggshell waste (4 %) and added water (9 %). Compared to methods using eggshell as an expanding agent producing cellular glass with low compression strength, the technique adopted by the authors is original by the addition of sodium borate, which contributes to increasing the compression strength and the use of the unconventional electromagnetic wave heating method, which ensures very economical specific energy consumption. The optimal variant of cellular glass had the following characteristics: density of 0.40 g/cm3, porosity of 81 %, heat conductivity of 0.086 W/m·K, compression strength of 4.3 MPa and the cell dimension between 0.3-0.9 mm. The specific energy consumption of the process was 0.80 kWh/kg. The product has adequate features for using as a heat insulation material under conditions of quite high mechanical loading.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.