Abstract
In the current investigation, TEM in-situ heavy ion (1 MeV Kr2+) irradiation with helium pre-injected at elevated temperature (400 °C) was conducted to simulate in-reactor neutron irradiation induced damage in CANDU spacer material Inconel X-750, in an effort to understand the effects of helium on irradiation induced cavity microstructures. Three different quantities of helium, 400 appm, 1000 appm, and 5000 appm, were pre-injected directly into TEM foils at 400 °C. The samples containing helium were then irradiated in-situ with 1 MeV Kr2+ at 400 °C to a final dose of 5.4 dpa (displacement per atom). Cavities were formed from the helium injection solely and the cavity density and size increased with increasing helium dosage. In contrast to previous heavy ion irradiations with cold pre-injected helium, heterogeneous nucleation of cavities was observed. During the ensuing heavy ion irradiation, dynamical observation showed noticeable size increase in cavities which nucleated close to the grain boundaries. A “bubble-void” transformation was observed after Kr2+ irradiation to high dose (5.4 dpa) in samples containing 1000 appm and 5000 appm helium. Cavity distribution was found to be consistent with in-reactor neutron irradiation induced cavity microstructures. This implies that the distribution of helium is greatly dependent on the injection temperature, and helium pre-injection at high temperature is preferred for simulating the migration of the transmutation produced helium.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.