Abstract
Catalytic wet peroxide oxidation of phenol over AlFe-pillared montmorillonite was carried out at room temperature, in a glass batch reactor, under constant airflow at day and UV light, alternatively. At higher concentration of phenol in water solution the efficiency of heterogeneous pillared clay catalyst was significantly lower than the efficiency of homogeneous iron catalyst.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.