Abstract
The landfill leachate was treated by catalytic wet oxidation. The catalysts was prepared by impregnation method, and FSC was used as catalyst carrier. Fe and Co were used as catalyst active components and Ce was used as catalyst auxiliary, and noble metal ruthenium was added to prepare supported multi-component composite catalyst of Fe-Co-Ru-Ce/γ-Al2O3. The water sample pH, decolorization rate, COD removal rate and turbidity removal rate were used as evaluation indexes of catalyst activity. The catalysts were prepared under the conditions of calcination temperature of 450 °C and calcination time of 3 h. Under the same conditions, for the Landfill Leachate, the COD removal rate, decolorization rate, turbidity removal rate of the water samples reached 78.1%, 60.4% and 92.7%, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.