Abstract

Au was loaded (1% wt.) on three different ZnO supports, by three different methods: photodeposition, double impregnation and ultrasonication. Two commercial ZnO supports were used, along with a ZnO sample consisting of nanosized single crystals prepared by chemical vapour deposition. The samples were extensively characterised by various techniques. CO oxidation was used as a test reaction to compare the catalytic activity. The best results were obtained with ZnO prepared by chemical vapour deposition with Au loaded by ultrasonication that showed an activity of 2 mol CO g Au - 1 h - 1 at room temperature. High-resolution electron microscopy images of the sample showed a number of gold nanocrystals epitaxially oriented on the ZnO rod. The unique catalyst–substrate interaction can be related to the increased catalytic activity of this sample, which was not observed for any of the others.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.