Abstract

Catalytic partial oxidation (CPOx) of n-butane in O 2/Ar mixtures at ratios of 1/3.76 has been investigated over Rh catalysis impregnated in γ-Al 2O 3 washcoat supports coated on α-Al 2O 3 ceramic foam monoliths. The impact of heat loss on Rh-based CPOx reactor performance for small-scale SOFC application is tested here by varying reactor lengths, insulation, and flow conditions. Results for a C/O ratio = 1.0 and T in = 300 °C indicate the n-butane conversion and H 2 and CO selectivity depend strongly upon reactor temperature and thus heat lost through the external reactor walls. Because heat loss does not scale with flow rate, higher flow rates for catalyst contact times approaching 15 ms increase fuel conversion and syngas selectivity. Furthermore, shortening catalyst length (from 10 to 5 mm) also reduces heat loss and increases fuel conversion and H 2 selectivity. CO selectivity, however, drops with the shorter length. These results suggest that for the conditions tested, butane conversion and H 2 production occur rapidly within the first couple of mm in the reactor, whereas CO production occurs more broadly throughout the reactor length. This study provides valuable insight into the conditions needed for good CPOx performance for fuel processing in small-scale SOFC applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.