Abstract

Abstract The degradation of polypropylene (PP) was carried out at 380 °C by batch operation using silica-alumina catalyst in 1) liquid phase contact and 2) vapor phase contact. For liquid phase contact, the liquid hydrocarbon products with a yield of 69 wt% had a boiling points (BP) range of 36 to 270 °C, equivalent to the BP of normal paraffins n-C6 to n-C15. For vapor phase contact, the yield of liquid products was much lower (54 wt%) and the rate of liquid recovery was much slower.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.