Quasi-aligned undoped ZnO nanorods with diameter in the range 100–300 nm and length of several micrometers have been grown catalyst-free on Si(1 0 0) wafer in a one-step process by direct heating of Zn powders. All nanowires are single crystals and are aligned vertically to the substrate surface with c-axis preferred orientation. XRD, HRTEM and Raman studies revealed that the ZnO nanorods have wurtzite phase, are highly crystalline and well aligned with the lattice parameters a=0.32 nm and c=0.52 nm. The PL spectra measured at different temperatures are dominated by excitonic emission at ∼380 nm and less intense below band gap emission band centered at 520 nm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.