Abstract

Detailed understanding of growth termination in vertically aligned single-walled carbon nanotubes (SWNTs) made via supergrowth, or water-assisted growth, remains critical to achieving the ultralong SWNTs necessary for next-generation applications. We describe the irreversible catalyst morphology evolution that occurs during growth, and which limits the lifetime of surface supported catalysts. Growth termination is strongly dependent on growth temperature, but not sensitive to C2H2:H2O ratio. In addition to both planar Ostwald ripening of small (sub-5 nm) Fe catalyst particles and diffusion of metal atoms into the alumina support, other features that contribute to growth termination or deceleration are described, including center-of-mass particle motions and coalescence of smaller species of surface supported Fe nanoparticles. Additionally, a temperature-induced structural transition in the alumina catalyst support is found to be coincident with abrupt growth termination at temperatures of 800 °C and higher. In situ electron microscopy observations are used to directly support these observations.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.