Abstract

Abstract The LiMgPO4 ceramic has been prepared through the solid state ceramic route. The powder has an average particle size of 1.1 μm and BET surface area of 2.7 m2 g−1. Good dispersion of LiMgPO4 has been achieved in ethanol/xylene mixture with the addition of 2 wt.% fish oil. The tape casting slurry of LiMgPO4 with typical pseudoplastic behavior has been prepared and cast into thin tapes of thickness 70 μm. LiMgPO4 green tape shows a tensile strength of 0.22 MPa and average surface roughness of 0.25 μm. The green tape has an ɛr of 3.2 and tan δ of 0.0688 at 5 GHz. The thermo-laminated tape (4 layers) sintered at 950 °C/2 h shows good microwave dielectric properties: ɛr = 6.4 and tan δ = 0.0002. LiMgPO4 has a coefficient of thermal expansion of 10.5 ppm/°C and thermal conductivity of 7.1 W m−1 K−1.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.