Abstract
In this study, α-Si3N4 powder was produced by carbothermal reduction and nitridation (CRN) of quartz from Can-Canakkale. Carbon with a specific surface area of 110 m2g−1 and quartz powders were mixed then the powder mix was placed in an alumina tube furnace and reacted in between 1300-1500°C for 4 hours under nitrogen flow. The quartz powder was carbothermally reduced and nitrided to form silicon nitride powders. XRD results showed that the reaction product was mainly α-Si3N4 and contained some β-Si3N4 and residual quartz. In order to reduce amount of unreacted quartz, the raw materials mixture was grinded either with carbon black or with no carbon. After CRN reactions of separate grinded quartz powders with carbon, residual quartz was disappeared, reaction temperature was decreased and α-Si3N4 rate was increased. Hence, a better mixing of carbon and fine silica enhanced the α phase formation. SEM images and XRD pattern showed that sub micron particles (0.6–0.87m), high α-phase content Si3N4 powders can be produced at 1450°C for 4 h in flowing nitrogen gas during the CRN process.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.