Abstract
The generation of carbonyl groups during sulfonation of porous styrene−divinylbenzene copolymers is reported. The carbonyl groups and sulfonic acid groups were verified by infrared spectroscopy and quantified by acid−base titrations. A gradual change in sulfonation reaction conditions from 70 °C/30 min to 98 °C/60 min resulted in a gradual increase in sulfonic acid group concentration from ∼1.85 to ∼3.13 mol/kg and in the carboxylic acid group concentration from ∼0 to ∼0.34 mol/kg. Data on the swelling coefficients in water indicate a slight increase in cross-linking during sulfonation. Conversion of ethyl or residual vinyl groups to carboxylic acid groups, followed by conversion of some of the acid groups to cross-links through an acid-catalyzed acylation reaction, is proposed. The proposed reactions also explain the pH-dependent color change of the resins. Sulfonation of copolymers with varied cross-linkages further supports our assertion that, as the concentrations of ethyl and residual vinyl groups increase, the concentration of —COOH groups also increases and the resin color becomes darker.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.