Abstract

Advanced lithium-ion batteries utilize high upper cut-off voltages up to 4.8V versus lithium metal to reach extraordinary energy densities. Such a harsh environment challenges the cathode stability and requires the construction of robust cathode electrolyte interphases at their electrochemical interface. Inspired by carbonated beverages with supersaturated CO2, here, a surface modification strategy that produces effective passivation layer of low modulus from the weakest link, is proposed CO2 bubbles preferentially nucleate and grow at rough surfaces, which in oxide cathodes, are also the local regions offering fast degradation pathway. Metal ion exchange on carbonated layer assists the construction of highly elastic interface under the guidance of packing factor. This method enables surface reconstruction at both primary and secondary particle levels for various cathodes exemplified by high-voltage LiNi0.8Co0.1Mn0.1O2 (NCM811) and LiCoO2 (LCO). Remarkably, with ultra-high upper cut-off voltage of 4.8V versus Li+/Li, over 235 mAh g-1 discharge capacity, and over 900W h kg-1 discharge energy at cathode level, ≈90% capacity retention can be obtained for LiNi0.8Co0.1Mn0.1O2 over 100 cycles at 0.5 C with commercial carbonate electrolytes. This carbonated beverage chemistry is promising for constructing high-quality surface passivation in many extreme-condition applications beyond battery cathodes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.