Abstract
Carbon encapsulated magnetic nanoparticles (CEMNs) were synthesized by heating an aqueous glucose solution containing Fe–Au (Au coated Fe nanoparticles) nanoparticles at 160–180 °C for 2 h. This novel hydrothermal approach is not only simple but also provides the surface of CEMNs with functional groups like OH. The formation of carbon encapsulated magnetic nanoparticles was not favored when using pure Fe nanoparticles as cores because of the oxidation of Fe nanoparticles by H 2O during the reaction and, therefore, the surfaces of the naked Fe nanoparticles had to be coated by Au shell in advance. TEM, XRD, XPS and VSM measurments characterized that they were uniform carbon spheres containing some embedded Fe–Au nanoparticles, with a saturation of 14.6 emu/g and the size of the typical product is ∼350 nm.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.