Abstract
Physicochemical phase analysis is used to investigate carbide phases in a high-temperature nickelbased alloy ZhS32 after the alloy has been subjected to various heat treatments and aging regimes within a temperature range of 850–1250°C. The MC, M23C6, and M6C carbide phases have been identified.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.