Abstract
Reliable thermophysical data of Ni-based superalloys are needed for the mathematical modelling of solidification in casting applications. This paper derives equations and procedures to calculate the following properties of these alloys from chemical composition of the alloy: the γ′ phase content, liquidus and solidus temperatures, density and thermal expansion coefficient, heat capacity and enthalpy, electrical resistivity, thermal diffusivity and conductivity, viscosity, surface tension and contact angle. Estimates are also for the diffusion coefficient and emissivity. This work has revealed an urgent need for reliable property measurements on liquid Ni-based alloys for the following: heat capacity, electrical resistivity, thermal diffusivity and conductivity, emissivity and diffusion coefficients.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.