Abstract

In this paper, we have reported the thermoluminescence (TL) glow curves and kinetic parameters, activation energy; order of kinetics, frequency factor of (Zn, Cd)S mixed phosphor under UV irradiations. The sample was prepared by solid state reaction method, thereafter the TL glow curves were recorded for different doses of UV exposure at heating rate 10°C s−1. The sunthesized phosphor exhibit the TL glow peaks at 136°C for heating rate 10°C s−1 at different doses 5 min; 10 min; 15 min of UV exposure. The kinetic parameters activation energy E; order of kinetics b; frequency factor S of synthesized phosphor have been calculated by using peak shape method and also calculated the trap depth was determined using different formula. Here prepared phosphor shows linear response with dose so we interpreted that these is may be useful for dosimetric material. Also the TL glow curve recorded for different heating rate 2 to 10°C s−1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.