Abstract

According to regulatory documents, welding can be performed at ambient temperatures from minus 15 ° C to plus 45 ° C. When laying gas pipelines at a lower outside temperature, it is necessary to organize their heating to the required temperature. In this case, the temperature of the heated air should not be more than plus 60 ° C. If you start working with a polyethylene (PE) pipe at low temperatures, then the PE pipe will have completely different characteristics. The weld seam may not be reliable.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.