Abstract

The reduction of zirconium dioxide using liquid calcium and molten calcium chloride was investigated. The study focusing on the influence of reductant amount, reaction time, CaCl 2 amount, and temperature on the reduction process. Zirconium powder with oxygen content less than 800 ppm was obtained at 1 100ยฐC after 3 h and by using two times the theoretical amount of Ca and four times that of CaCl 2 . The reduction reaction of ZrO 2 was found to be multi steps process through the formation of intermediate phase CaZrO 3 . The morphology of the obtained zirconium was observed to be highly affected by the reaction temperature.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.