Abstract

Purpose: Fracture strength of all-ceramic 3-unit fixed partial dentures manufactured by CAD/CAM and copymilling systems were evaluated. Methods: Zirconia cores were made by milling the pre-sintered zirconia block by CAD/CAM or copy milling method followed by subsequent sintering. By building-up the corresponding porcelains on the core, all-ceramic bridges were fabricated, and those were evaluated in comparison with PFM fixed partial denture. Results: During the flexural test of the 3-unit PFM bridge, the porcelain started to chip or break at 507.28( 62.82)kgf and the metal framework did not break until the maximum load level of 800kgf which was set in the testing instrument of this study. However, among all-ceramic restoration test groups, Everest(EV) group showed a peeling off or breakage of the porcelain from 365.64( 64.96)kgf and the core was broken at 491.77( 55.62)kgf. Those values of Zirkonzahn(ZR) were 431.03( 58.47)kgf and 602.74( 48.44)kgf, respectively. The break strength of the porcelain of PFM(PM) group was significantly higher than that of EV (p 0.05). ZR group showed higher break strength than that of EV group however there was no significant difference (p>0.05). The break strength of cores were in the increasing order of EV 0.05). [Abstract]

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.