Abstract

• Al 75 V 12.5 Fe 12.5 − x Cu x ( x = 0, 6.25, and 12.5 at%) amorphous powders were synthesized by MA. • Bulk Al 75 V 12.5 Fe 12.5 amorphous alloy is obtained by means of hydraulic pressing. • The Vickers microhardness of bulk sample is in the range of 821-927 HV. Hydraulic press was used to produce bulk amorphous Al 75 V 12.5 Fe 12.5 − x Cu x ( x = 0, 6.25, and 12.5) (at.%) alloy by consolidation of mechanically alloyed amorphous powder. The as-milled powders and bulk alloy were examined by X-ray diffraction, transmission electron microscopy and differential scanning calorimetry. The glass-forming ability was evaluated in accordance with the milling time. The results show that the glass-forming ability of the mechanical-alloyed Al 75 V 12.5 Fe 12.5 − x Cu x powders decreases with the increase of x . The onset crystallization temperatures ( T x onset ) of the three powders are 749 K, 771 K and 712 K, respectively. The results also indicate that the quality of consolidation is very good and the product’s Vickers microhardness is relatively high (821–927 HV).

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call