Bulge testing using a pressurized fluid to fracture the interface between bonded material layers along with three-dimensional digital image correlation to measure the sample distortion caused by pressurized fluid was applied to plasma-sprayed coatings. The initiation fracture toughness associated with the bonded materials was measured during the testing. The bulge testing of the uranium-molybdenum alloy plasma sprayed with zirconium and clad in aluminum is presented. The initiation fracture toughness was observed to increase with the increasing cathodic arc-cleaning current and the use of alternating polarity transferred arc current. This dependence was linked to the interface composition of oxide and mixed metal phases along with the interface temperature during spray deposition.