Abstract

Being the first step of foaming, bubble heterogeneous nucleation of aluminum foam has remarkable effects on the final cell structure of aluminum foam. The bubble heterogeneous nucleation of foaming Al-9Si and TiH2powder compact has been analyzed. The results obtained are given as follows: (1)The remaining TiH2particles act as the nuclei during heterogeneous nucleation. (2)The nucleation rate increases with the increasing of TiH2content, the decrease of TiH2granularity, the elevation of foaming temperature, and the elongation of foaming time. (3) Only about 5‰ bubble nuclei can survive and develop to the final foam cells. (4)The influence of processing parameters on the nucleation rate descends by the following sequence: foaming temperature elevates 20°C, TiH2granularity decreases from 150μm to 26μm, TiH2content increases 0.5%wt., and the time for foaming extends 10s.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.