In this work, we proposed a feasible method to prepare the Bi/Al co-doped silica glass by using laser additive manufacturing technology. Bi was uniformly doped into the silica matrix. The hydroxyl content of the glass sample was measured to be 29.36 ppm. Using an 808 nm laser diode as the excitation source, a broadband near-infrared emission from 1000 to 1600 nm was obtained. The emission peak was centered at 1249 nm, and the corresponding FWHM was more than 400 nm. The results show that the laser additive manufacturing technology is promising to fabricate highly homogeneous Bi-doped core materials with broader emission band, which is beneficial to solving the communication capacity crunch and promotes the development of fiber communication in the upcoming fifth and sixth generation systems.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.