AbstractThe brittle failure of saline columnar ice was investigated under biaxial compression at and −10° and −40°C over the range 0 ≤ RA < 1 where RA is the ratio of the intermediate to major principal compressive stress. The major principal stress and the intermediate (confining) stress were orthogonal to the columnar axes (type-A confinement); both stresses and the c-axes of the grains were co-planar. The results confirm earlier work by Hausier (1981) and Timco and Frederking (1983, 1986) on saline ice and follow similar behavior to fresh-water columnar ice found by Smith and Schulson (1993) and Frederking (1977). Failure stress and failure mode are sensitive to the confinement and two regimes of behavior are found: the failure stress first rapidly increases with RA in the range 0 ≤ RA < RT and then tends to decrease for RA > Rt. The transition stress ratio, Rt changes from ≈0.2 at −10°C to ≈0.1 at −40°C. The failure mode changes from axial splitting to shear faulting in the loading plane for 0 < RA < Rt. Above Rt failure changes to a combined mode of splitting across the columns and shear faulting out of the loading plane. The failure-stress envelope is of a truncated Coulomb-type. Damage studies show wing cracks and local fragmentation of grains involving the brine pockets. The results are explained in terms of Coulombic sliding and Hertzian crack mechanics.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call