Abstract

CaBi4Ti4O15 (CBTi144) micro-plateaus were fabricated on Si wafers and Pt foils using a self-assembled monolayer (SAM) and a complex metal alkoxide solution. The micro-plateaus are delineated by metal masks, which are used for shadowing against the ultraviolet (UV) irradiation for decomposition of SAM to make the surface hydrophilic. The micro-plateaus crystallized to a ferroelectric phase with random orientation. The crystallization depended on the SAM-derived ultra thin layers at the surface of the substrates. The primitive PFM measurements without any top electrodes confirmed that the micro-plateaus exhibited the piezoresponse behaviors. The piezoelectric constant, d33, had some distribution, and the maximum d33 was confirmed as about 45 pm/V, which is identical to the d33 of the polar-axis oriented CBTi144 thin films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.