Three natural type IIa diamond crystals were used for forced diffusion of boron. The diffusion was performed under bias otherwise with the same conditions. The boron diffusion coefficient in diamond was found to be 8.4 × 10−15 and 4 × 10−14 cm2/s at 1000 °C, depending on the direction of the electric field. The drift velocity of boron in diamond under 850 V at 1000 °C was found to be about 1.2 × 10−8 cm/s.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.