Abstract

Engineering liquid electrolytes for lithium (Li)-metal electrodes has been used to control the morphology of deposited Li in Li-metal batteries (LMBs). However, the Li corrosion problem remains unresolved, hindering the design of lean electrolytes for practical LMBs, which require the electrolyte/capacity (E/C) ratio to be 2 g Ah−1 or lower. Here we report a borate–pyran-based electrolyte to address the chronic Li-corrosion problem. We discovered that the borate–pyran electrolyte transforms large LiF crystallites in the solid–electrolyte interphase into fine crystalline or glassy LiF, which enhances the passivity of the Li/electrolyte interface by minimizing the permeation of electrolyte molecules into the solid–electrolyte interphase. LMBs assembled with the borate–pyran electrolyte, a high-nickel layered oxide cathode (3.83 mAh cm−2) and thin lithium (20 μm) delivered a high initial full-cell-level energy density (>400 Wh kg−1) and operated for 400 cycles with 70% capacity retention at an E/C ratio of 1.92 g Ah−1, 350 cycles with 73% capacity retention at 1.24 g Ah−1 and 200 cycles with 85% retention at 0.96 g Ah−1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.