Ce3+-activated lanthanide silicon oxynitride (La5Si3O12N, La4SiO7N2, LaSiO2N, and La3Si8O4N11) phosphors were prepared by firing the mixture of La2O3, Si3N4, SiO2, and CeO2 at 1500–1600 °C under a 0.5 MPa nitrogen atmosphere. Diffuse reflection spectrum, photoluminescence spectra, and temperature-dependent luminescence of these phosphors are presented in this work. A blue emission of Ce3+ in all lanthanide silicon oxynitrides was observed under ultraviolet irradiation, which is strongest in La3Si8O4N11:Ce3+. The concentration quenching and thermal quenching of the samples were discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.