Abstract

Chromium and cobalt oxides are widely used in the manufacture of industrial pigments. In this work, the Co(Co 2− x Cr x )O 4 powders with different chromium concentrations ( x = 0, 0.25 and 1) were synthesized by the polymeric precursor method, heat treatment between 600 and 1000 °C. These powders were characterized by X-ray diffraction, infrared spectroscopy, colorimetry, UV–vis absorption and X-ray photoelectron spectroscopies. Even with the addition of chromium, the XRD patterns revealed that all powders crystallize in a single spinel cubic structure. The spinels with higher cobalt amount, Co(CoCr)O 4 and Co(Co 1.75Cr 0.25)O 4, displayed a dark color, without the Co 3+ reduction observed in Co 3O 4 between 900 and 950 °C. The spinel with higher chromium amount, CoCr 2O 4, was green. The colors were directly related to the occupation of tetrahedral and octahedral sites by the chromophores, as well as to the different oxidation states of chromium and cobalt. The different optical band gap values estimated from UV–vis spectra suggested the existence of intermediary energy levels within the band gap. X-ray photoelectron spectroscopy confirmed an increasing presence of Co(III) and a decreasing amount of Cr(VI) with cobalt enrichment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.