Elemental bismuth (Bi) exhibits a high magnetoresistance as a typical example of semimetal, which has significant application in information technologies. Silicate glass-clad Bi core fibers were fabricated by a molten core method and maintained core diameter of 100–150µm and overall diameter of 300–450µm. X-ray diffraction (XRD) and micro-Raman spectra showed the core to be highly crystalline with no observed secondary phases. Electro-probe micro-analyzer (EPMA) measurements confirmed a very well-defined core-clad interface. Demonstration of fibers with high magnetoresistance core materials and the potential integration with current state of the art technologies represents the first step in providing the building blocks for all-fiber sensors.