Abstract

The biomedical NiTi alloy was treated by micro-arc oxidation in an electrolytes containing sodium aluminate and sodium hypophosphite at 400 V constant voltages for 30 min. The MAO-treated NiTi has a porous microstructure on its surface and coatings consisting only of the γ-Al2O3 phase. The ceramic coating prepared by micro-arc oxidation is composed of Al, Ti, Ni, O, and P with the atomic concentration of 26.98%, 3.67%, 3.33%, 65.30% and 0.72%, respectively. The MAO-treated NiTi was soaked in a simulated body fluid (1.0SBF) to investigate the biomimetic deposition of apatite on the surface of Al2O3 coated NiTi alloy. It was found that Al2O3 coated NiTi alloy shows an excellent apatite-forming ability after soaking in a simulated body fluid (1.0SBF) for 14 days, while no apatite-forming ability was observed on bared NiTi alloy even though soaking time is up to 28 days.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.