Abstract

Bioleaching of arsenic (As)-rich, so-called “dirty” concentrates can produce additional Cu value from the flotation waste while simultaneously releasing toxic As. This study bioleached three such concentrates of varying pyrite/enargite ratios ([Py]/[Ena] = 0.7, 1.3 and 2.4) at a pulp density of 20%. The dissolution behavior of Cu and As in relation to the solution redox potential (Eh) was studied with and without activated carbon (AC) as a potential Eh-controlling catalyst. At this high pulp density, Eh was naturally suppressed, without a need for AC dosing, to <700 mV (a rapid pyrite dissolution is prevented in this Eh range). The effect of AC dosing on Eh varied depending on the type of concentrate; Eh was further reduced only in the case of the most enargite-rich concentrate, DC-I. Among the three concentrates, the highest Cu dissolution (35%) was seen in DC-I (without AC dosing), which simultaneously achieved the lowest As solubilization. Arsenic was immobilized as amorphous precipitates, likely in a mixture of ferric arsenate, cupric arsenate, basic ferric sulfate and sulfur. Arsenic immobilization became increasingly ineffective as the pyrite content increased in the concentrate. Based on these results, setting a lower [Py]/[Ena] ratio prior to the dirty concentrate bioleaching could be a useful approach to promote Cu dissolution and As immobilization simultaneously.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call