Abstract

Chitosan membrane possesses huge potential application in many fields, such as biomedicine, wastewater purification and environmental protection, however, the poor mechanical property restricts its further development. In this study, chitin whisker was prepared by hydrolysis method, and was firstly used as an interlayer to fabricate the multilayered chitosan membrane through layer-by-layer method, which is inspired by the natural materials' hierarchical structure. From the results of mechanical testing, it is shown that tensile strength of the multilayered chitosan membranes reaches up to 122.8MPa, which is about 2.5 times than that of neat chitosan membrane (i.e. 49.5MPa), and the elongation at break is sharply increased as well.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.