Abstract This study investigated the effect of the guar gum content on the degradation behavior of the polyester and polyether polyurethane acrylate composites under outdoor soil-burial exposure. Polyurethane acrylates-guar gum composites were characterized before and after soil degradation by Fourier transform infrared spectroscopy (FTIR), mechanical measurements and scanning electron microscopy (SEM). The results showed that the addition of guar gum produces significant improvement in the degradation rate of these composites. The guar gum filler’s susceptibility to humidity and to soil microorganisms resulted in significant chemical and morphological changes in the entire structure of the composite. Guar gum incorporation into the matrix of the crosslinked polyurethane acrylates leads to a significant decrease in the mechanical properties of the composite films after soil burial exposure.