Abstract

Poly(butylene succinate) (PBS)/jute composites were prepared, and the effects of fibre content, diameter, surface modification and arrangement forms on the biodegradability were evaluated by compost-soil burial test. The weight losses of PBS/jute composites are higher than that of pure PBS film and bulk jute fibre, and decreased with increasing fibre content. The weight loss of PBS/10% jute composite after 180 days is 62.5%. In the case of the effect of fibre diameter, the weight loss is found to decrease with decreasing fibre diameter. For the effect of fibre surface modification, the order of higher weight loss is PBS/untreated jute > PBS/alkali treated jute > PBS/coupling agent treated jute. Furthermore, the composite of PBS/woven fabric has the highest weigh loss, followed by that of PBS/nonwoven fabric and PBS/bulk jute fibre, respectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.