Biocoatings were formed on the surface of the Mg0.8Ca alloy by the method of micro-arc oxidation, in an electrolyte containing β-Ca3(PO4)2 (β-TCP) and CaSiO3, When the process voltage was varied in the range of 350–500 V, the thickness, roughness, and mass of the coatings increased to the values of 110 µm, 12 µm, and 11 mg, respectively. The presence of the following crystalline phases was determined in the coatings: α-TCP, wollastonite, forsterite and magnesium oxide. Coatings containing these compounds not only reduce the rate of bioresorption of the magnesium alloy, but also promote the process of bone tissue formation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.