Abstract

A new biodegradable nanocomposite was obtained from layer-by-layer (LBL) technique using highly deacetylated chitosan and eucalyptus wood cellulose nanowhiskers (CNWs). Hydrogen bonds and electrostatic interactions between the negatively charged sulfate groups on the whisker surface and the ammonium groups of chitosan were the driving forces for the growth of the multilayered films. The film growth was followed by UV-vis spectroscopy through the maximum value of the absorption band at 194 nm and showed the deposition of 14.7 mg.m(-2) of chitosan polymer in each cycle. Scanning electron microscopy showed high density and homogeneous distribution of CNWs adsorbed on each chitosan layer. Cross-section characterization of the assembled films indicates an average of approximately 7 nm of thickness per bilayer. The results presented in this work indicate that the methodology used can be extended to different biopolymers for the design of new biobased nanocomposites in a wide range of applications such as biomedical and food packaging.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.