Abstract

An ethanol (EtOH) solution of polymerized vinyltrimethoxysilane (VTMS), about 20-mers, was mixed with an aqueous solution of calcium acetate (Ca(OAc)2) and refluxed in N2 for 1 h to give sols of a typical composition VTMS : H2O : EtOH : Ca(OAc)2 = 1 : 9 : 8 : 0.05 (mol). Homogeneous films could be produced, by dip-coating, on Nylon6® and soda-lime glass, but not on polypropylene or polytetrafluoroethylene. The gel films did not deposit apatite within 14 days of soaking in a simulated body fluid whereas films abraded with emery paper as well as bulk gels deposited apatite on the surfaces within 7 days, indicating the present gel was suitable for bioactive coatings on Nylon6®

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.