Abstract
AbstractThe ability of powdered Nylon 612 to bind methyl orange, ethyl orange, propyl orange, and butyl orange was investigated at 5, 15, 25 and 35°C in an aqueous solution. The amount of binding of the dye is much higher with this polyamide than with powdered Nylon 66 reported previously,1 although the former polymer has fewer amide end groups. The Van't Hoff plots of the first binding constant for the binding of butyl orange and propyl orange by powdered Nylon 612 exhibit a bell‐shaped curve, whereas the plots for methyl orange and ethyl orange do not. Maximal binding occurs at approximately 15°C for propyl orange and at about 25°C for butyl orange. This is the first instance where the peculiar temperature dependence of the binding constant has been found in the binding of propyl orange, whose hydrophobicity is less than that of butyl orange. These tendencies can be accounted for in terms of increased hydrophobic of butyl orange. These tendencies can be accounted for in terms of increased hydrophobic domains in powdered Nylon 612 and enhanced hydrophobic contributions in the binding process.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Polymer Science Part A: Polymer Chemistry
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.