Jigging of the −2.8 +0.7-mm size fraction of a friable, low-grade manganese ore sample from Andhra Pradesh increased the Mn content of a concentrate by 7% to 8%, with an average recovery of 57%. The jig concentrate was mixed with the unjigged −0.7-mm size fraction and ground to −150 μm. The sample was then subjected to wet high-intensity magnetic separation (WHIMS). The magnetic fraction thus obtained showed an increase in Mn content of 6%, but with an overall recovery of only 50%. The results of hydrocyclone classification of −150-μm ground ore indicated that the method is not capable of upgrading the manganese content, as both ferromanganese oxides and aluminosilicate gangue minerals constitute the fine size fraction. However, when the nonmagnetic fraction obtained from the WHIMS of −150-μm ore is subjected to hydrocyclone classification and the underflow obtained is subjected to WHIMS again, an overall recovery of about 50% to 52% is obtained with at least a 7% to 8% increase in the Mn content of the product. The phosphorus content in the product is not reduced by either of the two combinations of methods. The complex association of phosphorus with all the major phases in the ore has been clearly demonstrated from the linear correlation between the distribution ratios of major constituent phases and phosphorus.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call